We characterized the interfaces of heterostructures with different stack sequences of La0.7Sr0.3MnO3/BiFeO3 (LSMO/BFO) and BFO/LSMO using TEM revealing sharp and rough interfaces, respectively. Magnetometry and magnetoresistance measurements do not show a detectable exchange bias coupling for the multistack with sharp interface. Instead, the heterostructures with rough and chemically intermixed interfaces exhibit a sizable exchange bias coupling. Furthermore, we find a temperature-dependent irreversible magnetization behavior and an exponential decay of coercive and exchange bias fields with temperature suggesting a possible spin-glass-like state at the interface of both stacks.
References
1.
R.
Ramesh
and N. A.
Spaldin
, Nat. Mater.
6
, 21
(2007
).2.
S. M.
Wu
, S. A.
Cybart
, D.
Yi
, J. M.
Parker
, R.
Ramesh
, and R. C.
Dynes
, Phys. Rev. Lett.
110
, 067202
(2013
).3.
P.
Yu
, J.-S.
Lee
, S.
Okamoto
, M. D.
Rossell
, M.
Huijben
, C.-H.
Yang
, Q.
He
, J. X.
Zhang
, S. Y.
Yang
, M. J.
Lee
, Q. M.
Ramasse
, R.
Erni
, Y.-H.
Chu
, D. A.
Arena
, C.-C.
Kao
, L. W.
Martin
, and R.
Ramesh
, Phys. Rev. Lett.
105
, 027201
(2010
).4.
P.
Yu
, Y. H.
Chu
, and R.
Ramesh
, Philos. Trans. R. Soc. London, Ser. A
370
, 4856
(2012
).5.
Q.
Xu
, Y.
Sheng
, X.
Xue
, X.
Yuan
, Z.
Wen
, and J.
Du
, Jpn. J. Appl. Phys., Part 1
53
, 08NM01
(2014
).6.
J.
Bertinshaw
, S.
Brück
, D.
Lott
, H.
Fritzsche
, Y.
Khaydukov
, O.
Soltwedel
, T.
Keller
, E.
Goering
, P.
Audehm
, D. L.
Cortie
, W. D.
Hutchison
, Q. M.
Ramasse
, M.
Arredondo
, R.
Maran
, V.
Nagarajan
, F.
Klose
, and C.
Ulrich
, Phys. Rev. B
90
, 041113(R)
(2014
).7.
S.
Singh
, J. T.
Haraldsen
, J.
Xiong
, E. M.
Choi
, P.
Lu
, D.
Yi
, X.-D.
Wen
, J.
Liu
, H.
Wang
, Z.
Bi
, P.
Yu
, M. R.
Fitzsimmons
, J. L.
MacManus-Driscoll
, R.
Ramesh
, A. V.
Balatsky
, J.-X.
Zhu
, and Q. X.
Jia
, Phys. Rev. Lett.
113
, 047204
(2014
).8.
M. J.
Calderón
, S.
Liang
, R.
Yu
, J.
Salafranca
, S.
Dong
, S.
Yunoki
, L.
Brey
, A.
Moreo
, and E.
Dagotto
, Phys. Rev. B
84
, 024422
(2011
).9.
R. F.
Neumann
, M.
Bahiana
, and N.
Binggeli
, Europhys. Lett.
100
, 67002
(2012
).10.
See supplementary material at http://dx.doi.org/10.1063/1.4941795 for details on deposition conditions, fabrication, MR measurements, and further structural and magnetic characterization.
11.
F.
Radu
and H.
Zabel
, Springer Tr. Mod. Phys.
227
, 97
(2008
).12.
S.
Brück
, G.
Schütz
, E.
Goering
, X.
Ji
, and K. M.
Krishnan
, Phys. Rev. Lett.
101
, 126402
(2008
).13.
B. D.
Cullity
, Introduction to Magnetic Materials
(Addison-Wesley
, Reading, MA
, 1972
).14.
N.
Moutis
, C.
Christides
, I.
Panagiotopoulos
, and D.
Niarchos
, Phys. Rev. B
64
, 094429
(2001
).15.
S.
Karmakar
, S.
Taran
, E.
Bose
, B. K.
Chaudhuri
, C. P.
Sun
, C. L.
Huang
, and H. D.
Yang
, Phys. Rev. B
77
, 144409
(2008
).16.
J. F.
Ding
, O. I.
Lebedev
, S.
Turner
, Y. F.
Tian
, W. J.
Hu
, J. W.
Seo
, C.
Panagopoulos
, W.
Prellier
, G.
Van Tendeloo
, and T.
Wu
, Phys. Rev. B
87
, 054428
(2013
).17.
X. H.
Huang
, J. F.
Ding
, G. Q.
Zhang
, Y.
Hou
, Y. P.
Yao
, and X. G.
Li
, Phys. Rev. B
78
, 224408
(2008
).18.
J. R. L.
de Almeida
and D. J.
Thouless
, J. Phys. A
11
, 983
(1978
).19.
D.
Sherrington
and S.
Kirkpatrick
, Phys. Rev. Lett.
35
, 1792
(1975
).20.
S.
Nakamura
, S.
Soeya
, N.
Ikeda
, and M.
Tanaka
, J. Appl. Phys.
74
, 5652
(1993
).21.
M. K.
Singh
, R. S.
Katiyar
, W.
Prellier
, and J. F.
Scott
, J. Phys.: Condens. Matter
21
, 042202
(2009
).22.
D.
Lebeugle
, D.
Colson
, A.
Forget
, M.
Viret
, A. M.
Bataille
, and A.
Gukasov
, Phys. Rev. Lett.
100
, 227602
(2008
).23.
S.
Han
and C. S.
Kim
, J. Appl. Phys.
113
, 17D921
(2013
).© 2016 AIP Publishing LLC.
2016
AIP Publishing LLC
You do not currently have access to this content.