High Resolution 3D Strain and Orientation Mapping within a Grain of a Directed Energy Deposition Laser Additively Manufactured Superalloy
Authors:
Y. Chen,
Y. T. Tang,
D. M. Collins,
S. J. Clark,
W. Ludwig,
R. Rodriguez-Lamas,
C. Detlefs,
R. C. Reed,
P. D. Lee,
P. J. Withers,
C. Yildirim
Abstract:
The industrialization of Laser Additive Manufacturing (LAM) is challenged by the undesirable microstructures and high residual stresses originating from the fast and complex solidification process. Non-destructive assessment of the mechanical performance controlling deformation patterning is therefore critical. Here, we use Dark Field X-ray Microscopy (DFXM) to non-destructively map the 3D intragr…
▽ More
The industrialization of Laser Additive Manufacturing (LAM) is challenged by the undesirable microstructures and high residual stresses originating from the fast and complex solidification process. Non-destructive assessment of the mechanical performance controlling deformation patterning is therefore critical. Here, we use Dark Field X-ray Microscopy (DFXM) to non-destructively map the 3D intragranular orientation and strain variations throughout a surface breaking grain within a directed energy deposition nickel superalloy. DFXM results reveal a highly heterogenous 3D microstructure in terms of the local orientation and lattice strain. The grain comprises $\approx$ 5$μ$m-sized cells with alternating strain states, as high as 5 $\times 10^{-3}$, and orientation differences <0.5° . The DFXM results are compared to Electron Backscatter Diffraction measurements of the same grain from its cut-off surface. We discuss the microstructure developments during LAM, rationalising the development of the deformation patterning from the extreme thermal gradients during processing and the susceptibility for solute segregation.
△ Less
Submitted 8 March, 2023;
originally announced March 2023.
-
A New Class of Alumina-Forming Superalloy for 3D Printing
Authors:
Joseph N. Ghoussoub,
Przemysław Klupś,
William J B. Dick-Cleland,
Kathryn E. Rankin,
Satoshi Utada,
Paul A. J. Bagot,
D. Graham McCartney,
Yuanbo T. Tang,
Roger C. Reed
Abstract:
A new class of crack-resistant nickel-based superalloy containing high $γ^\prime$ fraction is studied for the laser-powder bed fusion (L-PBF) process. The effects of the (Nb+Ta)/Al ratio is emphasised, a strategy that is shown to confer excellent low-temperature strength whilst maintaining oxidation resistance at high temperatures via stable alumina scale formation. The processability of the new a…
▽ More
A new class of crack-resistant nickel-based superalloy containing high $γ^\prime$ fraction is studied for the laser-powder bed fusion (L-PBF) process. The effects of the (Nb+Ta)/Al ratio is emphasised, a strategy that is shown to confer excellent low-temperature strength whilst maintaining oxidation resistance at high temperatures via stable alumina scale formation. The processability of the new alloys is characterised with respect to defect assessment by micro-focus x-ray computed tomography; use is made of a prototype turbine blade geometry and the heritage alloy CM247LC as a benchmark. In all cases, some processing-related porosity is present in thin wall sections such as the trailing edge, but this can be avoided by judicious processing. The cracking seen in CM247LC -- in solid-state, liquation and solidification forms -- is avoided. A novel sub-solvus heat treatment strategy is proposed which takes advantage of AM not requiring solutioning; super-solvus heat treatment is inappropriate since it embrittles the material by deterioration of the texture and coarsening of grain boundary carbides. The tensile strength of the new superalloy is greatest when the Nb+Ta content is highest and exceeds that of CM247LC up to $\sim$900$\,$$^\circ$C. The oxidation resistance is best when Al content is highest, and oxidation-assisted cracking resistance maximized when the (Nb+Ta)/Al ratio is balanced. In all cases these are equivalent or superior to that of CM247LC. Nevertheless, the creep resistance of the new alloys is somewhat inferior to that of CM247LC for which the $γ^\prime$, C, and B contents are higher; this implies a processing/property trade-off which requires further clarification.
△ Less
Submitted 1 November, 2021;
originally announced November 2021.
-
On the influence of alloy composition on the additive manufacturability of Ni-based superalloys
Authors:
Joseph N. Ghoussoub,
Yuanbo T. Tang,
William J B. Dick-Cleland,
André A. N. Németh,
Yilun Gong,
D. Graham McCartney,
Alan C. F. Cocks,
Roger C. Reed
Abstract:
The susceptibility of nickel-based superalloys to processing-induced crack formation during laser powder-bed additive manufacturing is studied. Twelve different alloys -- some of existing (heritage) type but also other newly-designed ones -- are considered. A strong inter-dependence of alloy composition and processability is demonstrated. Stereological procedures are developed to enable the two do…
▽ More
The susceptibility of nickel-based superalloys to processing-induced crack formation during laser powder-bed additive manufacturing is studied. Twelve different alloys -- some of existing (heritage) type but also other newly-designed ones -- are considered. A strong inter-dependence of alloy composition and processability is demonstrated. Stereological procedures are developed to enable the two dominant defect types found -- solidification cracks and solid-state ductility dip cracks -- to be distinguished and quantified. Differential scanning calorimetry, creep stress relaxation tests at 1000$^\circ$C and measurements of tensile ductility at 800$^\circ$C are used to interpret the effects of alloy composition. A model for solid-state cracking is proposed, based on an incapacity to relax the thermal stress arising from constrained differential thermal contraction; its development is supported by experimental measurements using a constrained bar cooling test. A modified solidification cracking criterion is proposed based upon solidification range but including also a contribution from the stress relaxation effect. This work provides fundamental insights into the role of composition on the additive manufacturability of these materials.
△ Less
Submitted 30 September, 2021;
originally announced September 2021.
-
Grain Boundary Serration in Nickel Alloy Inconel 600: Quantification and Mechanisms
Authors:
Yuanbo T. Tang,
Phani Karamched,
Junliang Liu,
Jack C. Haley,
Roger C. Reed,
Angus J. Wilkinson
Abstract:
The serration of grain boundaries in Inconel 600 caused by heat treatment is studied systematically. A new method based on Fourier transforms is used to analyse the multiple wave-like character of the serrated grain boundaries. A new metric -- the serration index -- is devised and utilised to quantify the degree of serration and more generally to distinguish objectively between serrated and non-se…
▽ More
The serration of grain boundaries in Inconel 600 caused by heat treatment is studied systematically. A new method based on Fourier transforms is used to analyse the multiple wave-like character of the serrated grain boundaries. A new metric -- the serration index -- is devised and utilised to quantify the degree of serration and more generally to distinguish objectively between serrated and non-serrated boundaries. By considering the variation of the serration index with processing parameters, a causal relationship between degree of serration and solution treatment/cooling rate is elucidated. Processing maps for the degree of serration are presented. Two distinct formation mechanisms arise which rely upon grain boundary interaction with carbides: (i) Zener-type dragging which hinders grain boundary migration and (ii) a faceted carbide growth-induced serration.
△ Less
Submitted 27 March, 2020;
originally announced March 2020.
-
The Kinetics of Primary Alpha Plate Growth in Titanium Alloys
Authors:
Abigail K Ackerman,
Alexander J. Knowles,
Hazel M. Gardner,
Andre A N Nemeth,
Ioannis Bantounas,
Anna Radecka,
Michael P. Moody,
Paul A. J. Bagot,
Roger C. Reed,
David Rugg,
David Dye
Abstract:
The kinetics of primary alpha-Ti colony/Widmanstatten plate growth from the beta are examined, comparing model to experiment. The plate growth velocity depends sensitively both on the diffusivity D(T) of the rate-limiting species and on the supersaturation around the growing plate. These result in a maxima in growth velocity around 40 K below the transus, once sufficient supersaturation is availab…
▽ More
The kinetics of primary alpha-Ti colony/Widmanstatten plate growth from the beta are examined, comparing model to experiment. The plate growth velocity depends sensitively both on the diffusivity D(T) of the rate-limiting species and on the supersaturation around the growing plate. These result in a maxima in growth velocity around 40 K below the transus, once sufficient supersaturation is available to drive plate growth. In Ti-6246, the plate growth velocity was found to be around 0.32 um min-1 at 850 oC, which was in good agreement with the model prediction of 0.36 um min-1 . The solute field around the growing plates, and the plate thickness, was found to be quite variable, due to the intergrowth of plates and soft impingement. This solute field was found to extend to up to 30 nm, and the interface concentration in the beta was found to be around 6.4 at.% Mo. It was found that increasing O content will have minimal effect on the plate lengths expected during continuous cooling; in contrast, Mo approximately doubles the plate lengths obtained for every 2 wt.% Mo reduction. Alloys using V as the beta stabiliser instead of Mo are expected to have much faster plate growth kinetics at nominally equivalent V contents. These findings will provide a useful tool for the integrated design of alloys and process routes to achieve tailored microstructures.
△ Less
Submitted 31 July, 2019; v1 submitted 24 May, 2018;
originally announced May 2018.